INSPECTION DURING AND IMMEDIATELY AFTER SYSTEM PRESSURE TESTS

WARNING: EXTREME CARE MUST BE EXERCISED WHILE INSPECTING ANY PRESSURIZED SYSTEM OR COMPONENT.

A visual inspection of the system shall include checking for the following.

  • Evidence of leakage or loss of pressure.

  • Distortion or yielding of anchors, expansion joint hardware, the bellows and other piping components.

  • Any unanticipated movement of the piping due to pressure.Evidence of instability (squirm) in the bellows.

  • The guides, expansion joints and other moveable parts of the system shall be inspected for evidence of binding.

  • Any evidence of abnormality or damage shall be reviewed and evaluated by competent design authority.


Design Specification and Expansion Joint Design
| Installation | Post Installation Inspection Prior to System Pressure Test | Inspection During and Immediately after System Pressure Tests| Periodic Inservice Inspection | System Operation | Typical Causes of Expansion Joint Failures





Home | Products | Services | Catalogs | Downloads | Technical | News | Site Map | Contact Us | Privacy Policy
Mailing: P.O. Box 34506, Houston, TX 77234-4506     Location: 3701 Holmes Road, Houston, TX 77051
Phone: (713) 731-0030          Toll Free: (800)787-5914          FAX: (713) 731-8640          E-MAIL: info@pipingtech.com

Copyright 2007  Piping Technology and Products, Inc. All Rights Reserved.
Emergency Quote Request Order Status